Charpy Impact Unnotched | 1.78 J/cm² @Temperature 23.0 °C |
8.47 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |