Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² @Temperature 23.0 °C |
0.952 - 1.43 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179/1eU |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179/1eU |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |