Polymer Property : Bend Radius, Minimum = 4.5 t Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Bend Radius, Minimum 4.5 t
4.5 t
t ≤ 1.8 mm
Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed
Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength ..
Bend Radius, Minimum 4.5 t

@Thickness 2.00 mm
4.5 t

@Thickness 0.0787 in
Typical; sheet
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet
Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades..
Bend Radius, Minimum 4.5 t
4.5 t
Typical; on 0.078 in (2 mm) sheet
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar
Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit..
Bend Radius, Minimum 4.5 t

@Thickness 2.00 mm
4.5 t

@Thickness 0.0787 in
Typical; sheet
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged
Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi..
Bend Radius, Minimum 4.5 t
4.5 t
Typical; on 0.078 in (2 mm) sheet
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy
Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm..
Bend Radius, Minimum 4.5 t

@Thickness 2.00 mm
4.5 t

@Thickness 0.0787 in
Typical; sheet
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA
Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, ..