Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | >= 1.8 t | >= 1.8 t | t>6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 550MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.8 t | >= 1.8 t | t>6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 1.8 t | >= 1.8 t | t>6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 600MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.8 t | >= 1.8 t | t>6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 640XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |