Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.85 J/cm² @Temperature -30.0 °C |
8.80 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |