Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 623 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 131 J/cm²

@Thickness 1.50 mm,
Temperature -40.0 °C
623 ft-lb/in²

@Thickness 0.0591 in,
Temperature -40.0 °F
Longitudinal
AK Steel 2205 Duplex Stainless steel
AK Steel 2205 provides a combination of high strength, excellent corrosion resistance and stress-corrosion cracking resistance as well as very good pitting resistance, and low thermal expansion. Th..
Copyright © lookpolymers.com All Rights Reserved