Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.02 J/cm² @Temperature 23.0 °C |
4.85 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |