Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.56 J/cm² @Temperature 22.8 °C |
36.0 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |