Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 69.3 J/cm² @# of Cycles 1.00 , Temperature -30.0 °C |
330 ft-lb/in² @# of Cycles 1.00 , Temperature -22.0 °F |
Transverse |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |