Polymer Property : Charpy Impact, Notched = 32.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 6.90 J/cm²

@Temperature -30.0 °C
32.8 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer
7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.