Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
conditioned; ISO 179-1eA
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex..
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c..
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech..
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnitel® PM650 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnitel® PM650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..