Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.730 J/cm² @Temperature -30.0 °C |
3.47 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSX (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |