Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.630 J/cm² @Temperature -30.0 °C |
3.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature -30.0 °C |
3.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature -30.0 °C |
3.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
PolyOne Bergamid™ B700 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature -30.0 °C |
3.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |