Mechanical Properties Metric English Comments
Charpy Impact, Notched 26.3 J/cm²

@Temperature 704 °C,
Time 3.60e+6 sec
125 ft-lb/in²

@Temperature 1300 °F,
Time 1000 hour
Special Metals INCONEL® alloy 693
INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t..