Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 71 T 15 PP, 15% mineral filling FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches - pack.. |
|||
Charpy Impact, Notched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 83 T 15 PP, 15% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 15% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Charpy Impact, Notched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa.. |