Polymer Property : Charpy Impact, Notched = 20.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
BASF Elastollan 695 AU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Charpy Impact, Notched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
BASF Elastollan 890 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Charpy Impact, Notched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
BASF Elastollan B 95 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..