Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.67 J/cm² @Temperature -30.0 °C |
12.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax ATE90-FN01N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |