Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.18 J/cm²

@Temperature -30.0 °C
10.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized
A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.