Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.290 J/cm² @Temperature -20.0 °C |
1.38 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A CP400 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® CST (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® CST 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-GM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |