Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.940 J/cm²

@Temperature 23.0 °C
4.47 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 MI/2 PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
Charpy Impact, Notched 0.940 J/cm²

@Temperature 23.0 °C
4.47 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
Charpy Impact, Notched 0.940 J/cm²

@Temperature 23.0 °C
4.47 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..