Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.598 J/cm² @Temperature 23.0 °C |
2.85 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |