Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.98 J/cm | 18.7 ft-lb/in | ASTM D256 |
Aclo Acculoy POL063L Polycarbonate PET Alloy |
|||
Izod Impact, Notched | 9.98 J/cm | 18.7 ft-lb/in | NB; ASTM D256 |
Solvay Engineered Polymers SEQUEL® E3000 HMS TPO