Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.29 J/cm | 9.91 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |