Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.25 J/cm @Temperature 0.000 °C |
9.84 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |