Mechanical Properties Metric English Comments
Izod Impact, Notched 9.70 J/cm

@Temperature 23.0 °C
18.2 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Kraton® FG1901 + PBT blend (30/70)
Blending KRATON FG polymers with PBT significantly improves the toughness. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second ..