Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.34 J/cm | 17.5 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 280 Nylon 6, High Impact A highly impact modified nylon 6 exhibiting excellent toughness and flexibility.Data provided by the manufacturer, Chem Polymer. |