Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.11 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
17.1 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |