Polymer Property : Izod Impact, Notched = 8.62 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.60 J/cm
8.62 ft-lb/in
ASTM D256
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Izod Impact, Notched 4.60 J/cm
8.62 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance. - Black: Ixef..
Izod Impact, Notched 4.60 J/cm
8.62 ft-lb/in
ASTM D256
Metton LMR M1534 Liquid Molding Resin
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce ..
Izod Impact, Notched 4.60 J/cm
8.62 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.