Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.34 J/cm | 15.6 ft-lb/in | ASTM D256 |
Braskem HB 0055 HDPE Blow Molding Polyethylene
(discontinued **) Applications: 200 liters L-ring drums. Information provided by Braskem |
|||
Izod Impact, Notched | 8.34 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
15.6 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Izod Impact, Notched | 8.34 J/cm @Thickness 3.17 mm |
15.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3027PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PJ is an extrusion grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 8.34 J/cm @Thickness 3.17 mm |
15.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3027PU(X) Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PU(X) is an extrusion grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 8.34 J/cm @Thickness 3.17 mm |
15.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3030PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3030PJ is a high viscosity gradeInformation provided by Samyang. |
|||
Izod Impact, Notched | 8.34 J/cm | 15.6 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N3040ST Nanoclay 4% Super Toughness Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |