Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.32 J/cm @Thickness 3.17 mm |
8.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.32 J/cm @Thickness 3.17 mm |
8.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.32 J/cm | 8.10 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 4.32 J/cm @Thickness 3.17 mm |
8.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |