Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.10 J/cm | 15.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East) Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold.. |
|||
Izod Impact, Notched | 8.10 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
15.2 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |