Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.90 J/cm | 14.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 7.90 J/cm | 14.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 7.90 J/cm @Temperature 23.0 °C |
14.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.90 J/cm | 14.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |