Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.374 - 4.21 J/cm | 0.700 - 7.89 ft-lb/in | Average value: 0.930 J/cm Grade Count:19 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |