Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 - 7.84532 J/cm @Temperature -40.0 - -20.0 °C |
1.87 - 14.6975 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 3.76 J/cm Grade Count:35 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Notched | 1.00 - 7.84532 J/cm @Thickness 1.57 - 6.40 mm |
1.87 - 14.6975 ft-lb/in @Thickness 0.0618 - 0.252 in |
Average value: 3.76 J/cm Grade Count:35 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |