Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.01 J/cm @Temperature 23.0 °C |
7.51 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |