Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.475 J/cm | 14.00 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer COPYLENE® CM005 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes..Applications: Extrusion, sheet, film.Infor.. |