Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 - 7.35 J/cm | 1.29 - 13.8 ft-lb/in | Average value: 2.38 J/cm Grade Count:55 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |