Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.71 J/cm | 6.95 ft-lb/in | Charpy Impact Strength, notched; ASTM D256 |
Diamond Polymers NPP25-0116 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |