Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.85 J/cm @Temperature 23.0 °C |
12.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched | 6.85 J/cm | 12.8 ft-lb/in | ASTM D256 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |