Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.75 J/cm | 12.6 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |