Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.38 J/cm @Temperature -30.0 °C |
12.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific) Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only. |