Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.24 J/cm @Thickness 6.35 mm |
6.06 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.24 J/cm @Thickness 6.35 mm |
6.06 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.24 J/cm | 6.06 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |