Polymer Property : Izod Impact, Notched = 6.03 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.290 - 6.03 J/cm
0.543 - 11.3 ft-lb/in
Average value: 1.10 J/cm Grade Count:126
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..