Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.230 - 5.82 J/cm | 0.431 - 10.9 ft-lb/in | Average value: 2.65 J/cm Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |