Polymer Property : Izod Impact, Notched = 40.00 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 21.35 J/cm

@Thickness 3.20 mm
40.00 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.