Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.86 J/cm | 9.10 ft-lb/in | Compression molded parts prepared according to ASTM D 1928, method A.; ASTM D256 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Izod Impact, Notched | 4.86 J/cm | 9.10 ft-lb/in | Compression molded parts prepared according to ASTM D 1928, method A.; ASTM D256 |
Dow CONTINUUM™ DGDC-2480 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |