Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® EX39F ABS Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant. |
|||
Izod Impact, Notched | 4.64 J/cm @Thickness 3.20 mm |
8.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2200 PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Izod Impact, Notched | 4.64 J/cm @Thickness 3.20 mm |
8.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2200 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Izod Impact, Notched | 4.64 J/cm @Thickness 3.20 mm |
8.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Izod Impact, Notched | 4.64 J/cm | 8.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |