Polymer Property : Izod Impact, Notched = 4.53 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.42 J/cm

@Temperature -30.0 °C
4.53 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® 123X PC Copolymer
Improved flow PC with excellent processability and mold release.
Izod Impact, Notched 2.42 J/cm

@Temperature -30.0 °C
4.53 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
Izod Impact, Notched 2.42 J/cm

@Temperature -30.0 °C
4.53 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.