Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.20 J/cm @Temperature -40.0 °C |
7.87 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.20 J/cm | 7.87 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |