Izod Impact, Notched 15.0 - 20.0 J/cm
28.1 - 37.5 ft-lb/in
IS 13411-1992
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en..